Add to Cart
Copper mould plate longer funels shortor funel thiner slabs thicker slab
Packaging Details
Standard seaworthy packing or as requirement
Delivery Time
1 month after order or as per customer's requirement
CuAg0.1 copper mould plate for CCM
1 A joint-venture
2 Meet EU standards
3 High efficency
4 Good thermal performance
Material Details:
ltem | Temp | Unit | Material | ||
CuDHP | CuAg0.1 | CuCrZr | |||
Mechanical properties | |||||
Ultimate tensile strength | 20 | Mpa | 240-310 | 240-310 | 375-445 |
Ultimate tensile strength | 100 | Mpa | 190-270 | 230-270 | 365-425 |
Ultimate tensile strength | 200 | Mpa | 140-190 | 205-240 | 365-410 |
Ultimate tensile strength | 300 | Mpa | 175-210 | 335-375 | |
Ultimate tensile strength | 400 | Mpa | 145-160 | 315-350 |
E-Cu | >99.90 | 200 | 40 | 40 | 45 | 98 | |
SF-Cu | >99.85 | P0.015-0.040 | 240-310 | 190-250 | 25-10 | 80-95 | 85 |
CuAg | >99.50 | Ag0.08-0.12 | 240-310 | 200-225 | 16-10 | 110-125 | 95 |
Cu-Cr-Zr | >98.0 | Cr0.3-1.2 Zr0.08-0.3 | 375-445 | 280-355 | 20-13 | 115-130 | 80 |
Chemical Composition | |||||
Cu 99.85 P0.015-0.040 | Cu 99.50 Ag0.08-0.12 | Cu 98 Cr 0.30-1.20 Zr 0.08-0.30 | |||
Physical properties | |||||
Electical conductivity | 20 | %IACS | 85 | 95 | 80 |
Thermal conductivity | 20 | W/(m.K) | 340 | 375 | 330 |
Coefficient of thermal expansion | 20-300 | 10^-6/K | 17.1 | 17.1 | 17.2 |
Recrystallisation temperature | ℃ | 345 | 360 | 690 | |
Modulus of elasticity | 20 | 10^3MPa | 120 | 123 | 126 |
Melting point | ℃ | 1083 | 1083 | 1078 | |